Total PPH 3862 Homopolymer Polypropylene, Fiber Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3862 Homopolymer Polypropylene, Fiber Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Total Petrochemicals Polypropylene 3862 is recommended for high speed melt spinning processes and multifilament yarns like bulk continuous filament (BCF) and continuous filament (CF) fibers. 3862 is specially designed for ultra fine staple fibers with good mechanical properties. 3862 features excellent processability and gas fade resistance in order to significantly reduce yellowing in fibers.3862 is also recommended for thin wall injection molding application requiring high fluidity and high stiffness or for compounding application.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Bulk Density 0.525 g/cc
0.0190 lb/in³
Internal
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Notched 0.170 J/cm
0.318 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ASTM D1525
Descriptive Properties Value Comments
Isotacticity Index (%) 96
Total Internal Test