Total PS CPDS 827 Flame Retardant Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Total Atofina
Trade Name PS CPDS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PS CPDS 827 Flame Retardant Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYSTYRENE (PS) COMPOUND (CPDS) 827 is a high impact flame retardant polystyrene for use in HGW applications. PS CPDS 827 can be supplied in both natural and colored forms.Main Characteristics:DBDPE and Antimony Trioxide free,Excellent UV stability,Hot Glow Wire rated to 750°CHigh flow.Applications: Insulated enclosures, Junction boxes.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527-2
Elongation at Break 39 %
39 %
ISO 527-2
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
180/1A
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C

@Load 5.10 kg
194 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
Glow Wire Test 750 °C
1380 °F
IEC 695-2-1
Processing Properties Metric English Comments
Melt Temperature <= 220 °C
<= 428 °F