Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo Pelprene™ P-30B Polyester TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Toyobo
Trade Name Pelprene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo Pelprene™ P-30B Polyester TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block copolymer consisting of an aromatic polyester as the hard segment and an aliphatic polyether as the soft one. It covers general purpose grades, being designed to have a balance of flexibility, heat & cold resistance, chemical resistance, and processability.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.58 %
0.58 %
25°C; 65%RH
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 2.00 mm
0.0040 in/in

@Thickness 0.0787 in
Melt Flow 14 g/10 min

@Temperature 190 °C
14 g/10 min

@Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Hardness, Shore D 29
29
ASTM D2240
Tensile Strength, Ultimate 7.00 MPa
1020 psi
ASTM D638
Elongation at Break 840 %
840 %
ASTM D638
50% Modulus 0.00250 GPa
0.363 ksi
ASMT D638
Flexural Modulus 0.0150 GPa
2.18 ksi
ASTM D790
Compressive Modulus 0.00196 GPa
0.284 ksi
10% Compression Modulus; ASTM D695
Resilience 78
78
JIS K6301
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 72.0 kN/m
411 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 20
20
CS-17 wheel; ASTM D1044
Compression Set 50 %

@Temperature 70.0 °C
50 %

@Temperature 158 °F
70°C; 22 hrs; JIS K6301
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
TMA
Melting Point 160 °C
320 °F
DSC
Vicat Softening Point 73.0 °C
163 °F
ASTM D1525
Brittleness Temperature -65.0 °C
-85.0 °F
JIS K6301
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Strength 20.0 kV/mm
508 kV/in
JIS K2111
Users viewing this material also viewed the following: