Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Bond 2138 Easy-Flow No-Sag Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 2138 Easy-Flow No-Sag Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 2138 epoxy adhesive is an easy-to-apply, room temperature cure epoxy adhesive system developed for structural bonding applications on vertical or overhead surfaces where its instant development of a no-sag characteristic is critical. This medium exotherming system exhibits excellent flow and wetting characteristics for precisely located dispensing from static mixing cartridges. Fully cured TRA-BOND 2138 may be employed on a wide variety of substrates including glass, most metals, and a variety of plastics and provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils and alcohol. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 33600 cP

@Temperature 25.0 °C
33600 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
24 hrs @ 25°C
75
75
1 hr @ 65°C
Adhesive Bond Strength 15.5 MPa
2250 psi
Lap shear, alum to alum, 24 hrs @ 25°C
25.0 MPa
3630 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 45.0 °C
113 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+13 ohm-cm
2.70e+13 ohm-cm
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 25 min
25 min
Descriptive Properties Value Comments
Color Amber
Mix Ratio, parts by weight 100/80
Resin/Hardener
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved