Tra-Con Tra-Bond FS279 Blush-Free Non-Sag Structural Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FS279 Blush-Free Non-Sag Structural Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FS-279 is a two-part epoxy adhesive specifically formulated to be non-sagging and have improved adhesion to smooth, non-porous substrates such as glass, ceramic, stainless steel, etc. This formulation has structural reinforcements which enhance its overall physical characteristics making it ideal for structural bonding applications. Fully cured TRA-BOND FS-279 provides excellent resistance to salt solutions, mild acids and alkalis and many other chemicals including petroleum solvents, lubricating oils and alcohols. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mixed
Viscosity 375000 cP

@Temperature 25.0 °C
375000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 65.0 °C
1.00 - 2.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Color Milky, Translucent
Mix Ratio, parts by weight 100/39
Resin/Hardener
Thixotropic Index 5.8
5 rpm/50 rpm