Trelleborg Emerson & Cuming Eccobond® 104 Two-Component High Temperature Performance Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 104 Two-Component High Temperature Performance Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 104 Eccobond® Two-Component High Temperature Performance Epoxy AdhesiveFilled, heat curing, high temperature resistant, epoxy adhesive. Excellent chemical resistance. Maintains high shear strength up to 230°C. Recommended for bonding metals, glass, ceramics and high temperature thermoset plastics. Mix ratio of 100:64. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 13.1 MPa
1900 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 120 °C
1.00 hour

@Temperature 248 °F
360 min

@Temperature 120 °C
6.00 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Color Black
Viscosity Thixotropic Paste