Material Notes:
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical properties by being able to acquire any targeted molecular structures. Specific Notes for this Grade: UMERIT® 2000F offers various excellent properties: Reduced motor load at processing, Draw resonance at high-speed drawing hardly occursInformation provided by UBE.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 1000 hour
1000 hour
F50; ASTM D1693
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
ASTM D2240
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 755 %
755 %
ASTM D638
Tensile Modulus 0.280 GPa
40.6 ksi
Bending Modulus; ASTM D790
Thermal Properties Metric English Comments
Melting Point 116 °C
241 °F
UBE method
Vicat Softening Point 104 °C
219 °F
ASTM D1525