Unipetrol PE HD LITEN® MB/ML 47 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Unipetrol RPA
Trade Name PE HD LITEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PE HD LITEN® MB/ML 47 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made for injection molding and special applicationsInformation provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 2.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
9.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 868
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Flexural Modulus 0.800 GPa
116 ksi
ISO 178
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
ISO 306