Material Notes:
Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.0 MPa
4210 psi
ISO 527
Elongation at Break 50 %
50 %
ISO 527
Flexural Modulus 1.55 GPa
225 ksi
ISO 178
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ISO 75
Vicat Softening Point 153 °C
307 °F
ISO 306
Users viewing this material also viewed the following: