Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Thermal Properties Metric English Comments
Heat Distortion Temperature >= 220 °C
>= 428 °F
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D149
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
ASTM D257
Descriptive Properties Value Comments
Color Yellow