Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Washington Penn PPH2CF2 Polypropylene, 20% Calcium Carbonate Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer Washington Penn
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn PPH2CF2 Polypropylene, 20% Calcium Carbonate Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer. FDA for food contact, anti-stat package included.Applications: Toys, appliances, housewares, and automotive components.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
50 cm/min; ASTM D638
Elongation at Break 300 %
300 %
at 50 cm/min; ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.500 J/cm

@Thickness 3.17 mm
0.937 ft-lb/in

@Thickness 0.125 in
ASTM D256
Gardner Impact 9.00 J
6.64 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648