Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Washington Penn
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Applications: AC Blower wheels, parts and appliances.Data provided by Washington Penn Plastic Co., Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ASTM D955
Melt Flow 3.0 - 7.0 g/10 min
3.0 - 7.0 g/10 min
Cond L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
50 cm/min; ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.300 J/cm

@Thickness 3.17 mm
0.562 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM D648