Material Notes:
Applications: liners, thrust shoes, bushings, cages and other valve components for nuclear applicationsInformation provided by Weartech International
Physical Properties Metric English Comments
Density 8.14 g/cc
0.294 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 45 - 56
45 - 56
Hardness, Vickers 100

@Treatment Temp. 760 °C
100

@Treatment Temp. 1400 °F
250

@Treatment Temp. 649 °C
250

@Treatment Temp. 1200 °F
450

@Treatment Temp. 427 °C
450

@Treatment Temp. 800 °F
480

@Treatment Temp. 538 °C
480

@Treatment Temp. 1000 °F
525

@Treatment Temp. 25.0 °C
525

@Treatment Temp. 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 15.1 µm/m-°C
8.40 µin/in-°F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Melting Point <= 1070 °C
<= 1950 °F
Liquidus 1070 °C
1950 °F
Component Elements Properties Metric English Comments
Boron, B 3.0 %
3.0 %
Carbon, C 0.60 %
0.60 %
Chromium, Cr 13 %
13 %
Iron, Fe 4.0 %
4.0 %
Nickel, Ni 75.7 %
75.7 %
Silicon, Si 3.7 %
3.7 %
Descriptive Properties Value Comments
Relative Wear Performance Cold Abrasion
Excellent
Corrosion
Good/Moderate
Erosion
Good/Moderate
Hot Abrasion
Good/Moderate
Impact
Not Recommended
Metal to Metal
Excellent
Copyright © lookpolymers.com All Rights Reserved