Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | RT |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Industeel Superplast® 400 High Hardness Mold Steel SUPERPLAST® 400 is an injection plastic mold steel pre-hardened to a high level of hardness. It is delivered at a typical hardness of 125 kg/mm2. This steel is specially adapted for heavy-duty .. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Latrobe LSSâ„¢ 17-4 Precipitation Hardening Stainless Steel (ASTM Type 360) TLS 17-4 is a precipitation hardening, martensitic stainless steel that exhibits excellent resistance to atmospheric and chemical corrosion. TLS 17-4 exhibits an excellent combination of high stren.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel TENASTEEL® Cold Work Tool Steel Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Weartech International WT-50 Nickel Hardfacing & Wear Resistant Alloy Applications: liners, thrust shoes, bushings, cages and other valve components for nuclear applicationsInformation provided by Weartech International |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
EDRO #7 Shock Resistant S7 Tool Steel EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 416R Chromium Stainless Steel Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific req.. |
|||
Specific Heat Capacity | 0.460 - 0.602 J/g-°C @Temperature 22.2 - 699 °C |
0.110 - 0.144 BTU/lb-°F @Temperature 72.0 - 1290 °F |
|
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 62 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 10 SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Chromium-molybdenum-vanadium alloyed steelUddeholm Vanadis 10 is a high vanadium alloyed powder metallurgy tool steel offering a unique combination of an excellent abrasive wear resistance in combin.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Assab Steels ASSAB XW-41 Cold Work Steel XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Assab Steels 718HH Plastic Mold Material IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Latrobe LSS™ 440C Stainless Steel Knife (ASTM A276) TLS 440C Stainless Knife Steel is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 60 HRC. The high carbon content results in a hard matrix and numero.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |