Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-93
Elongation at Break 35 %
35 %
ISO 527-93
Flexural Strength 95.0 MPa
13800 psi
ISO 178-93
Flexural Modulus 2.90 GPa
421 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75-93