Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183-87
Filler Content 10 %
10 %
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-93
Elongation at Break 7.0 %
7.0 %
ISO 527-93
Flexural Strength 120 MPa
17400 psi
ISO 178-93
Flexural Modulus 3.20 GPa
464 ksi
ISO 178-93
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75-93
Users viewing this material also viewed the following: