Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GS1791-N2 5% Glass Sphere Reinforced, Natural Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Bead Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GS1791-N2 5% Glass Sphere Reinforced, Natural Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Sphere Reinforced, Natural Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183-87
Filler Content 5 %
5 %
Linear Mold Shrinkage 0.018 - 0.028 cm/cm
0.018 - 0.028 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 105 MPa
15200 psi
ISO 178-93
Flexural Modulus 3.00 GPa
435 ksi
ISO 178-93
Izod Impact, Notched (ISO) 2.60 kJ/m²
1.24 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-93