Material Notes:
Description: General Purpose Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527-93
Elongation at Break 20 %
20 %
ISO 527-93
Flexural Strength 110 MPa
16000 psi
ISO 178-93
Flexural Modulus 2.80 GPa
406 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-93