Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Bead Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Sphere Filled, Toughened Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183-87
Filler Content 25 %
25 %
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 63.0 MPa
9140 psi
ISO 527-93
Elongation at Break 20 %
20 %
ISO 527-93
Flexural Strength 100 MPa
14500 psi
ISO 178-93
Flexural Modulus 3.20 GPa
464 ksi
ISO 178-93
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO 75-93
Users viewing this material also viewed the following: