Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.011 - 0.017 cm/cm | 0.011 - 0.017 in/in | ASTM D955 |
PolyOne Gravi-Tech™ GRV-PS-027-BA-WHT Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | ASTM D955 |
PolyOne Nymax™ 1200 A Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | ASTM D955 |
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE) Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | ASTM D955 |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.017 cm/cm | 0.0090 - 0.017 in/in | ASTM D955 |
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE) Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE) Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE) Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Faradex MS003XXC PP (Europe-Africa-Middle East) LNP* Faradex* MS003XXC is a compound based on Polypropylene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.This data was supplied by SABIC-IP for.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm @Thickness 3.17 mm |
0.013 - 0.017 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm @Thickness 3.20 mm |
0.013 - 0.017 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | |
LATI Latiblend 5262 PP Homopolymer/PA6 Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RN001XXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RN001XXC is a compound based on Nylon 66 resin containing MOS2. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.017 cm/cm | 0.012 - 0.017 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East) VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm @Thickness 3.20 mm |
0.013 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm @Thickness 3.20 mm |
0.014 - 0.017 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LH-XE-NBK1 Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-NBK2 Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® MR409 22H-GY1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylon® N2200 HL Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackProcessing Method: Injection MoldingInformation pr.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.017 cm/cm | 0.014 - 0.017 in/in | |
LATI Latishield 52/5-07A PP Homopolymer, Steel Fiber Reinforced EMI shielding product based on Polypropylene homopolymer (PPh). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.017 cm/cm @Thickness 3.50 mm |
0.015 - 0.017 in/in @Thickness 0.138 in |
ASTM D955 |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | |
Solvay TECHNYL® 1015CR PA6, DRY Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |