Material Notes:
Westlake LF2018 is a hexene LLDPE suitable for heavy duty films and shipping sacks. This material has increased stiffness, and can be blended with LDPE for strength property enhancements..Application/UsesHeavy duty bags and sacksAgricultural filmsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 1100 %
1100 %
ASTM D882
Film Elongation at Break, TD 1100 %
1100 %
ASTM D882
Dart Drop 11.8 g/micron
300 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 42.1 MPa
6100 psi
ASTM D882
Film Tensile Strength at Break, TD 37.2 MPa
5400 psi
ASTM D882
1% Secant Modulus, MD 283 MPa
41000 psi
ASTM D882
1% Secant Modulus, TD 372 MPa
54000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 204 - 216 °C
400 - 420 °F
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution