Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Lennite® Ultra High Molecular Weight Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Westlake Plastics
Trade Name Lennite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Lennite® Ultra High Molecular Weight Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lennite UHMW-PE is a low friction engineering plastic with excellent chemical resistant and abrasive wear resistance. It is widely used in conveyors, packaging machinery, and food processing machinery since it is inherently low friction, wears well, and is not abrasive to mating parts. Westlake manufactures Lennite with extremely low levels of residual stress so it can be machined into complex parts with minimal deformation. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Water Absorption 0.00 %
0.00 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength at Break 41.4 MPa
6000 psi
ASTM D638
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Elongation at Break >= 350 %
>= 350 %
ASTM D638
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D256; Double 15° Notch at 73°F
Thermal Properties Metric English Comments
CTE, linear 198 µm/m-°C

@Temperature 20.0 °C
110 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.3

@Frequency 60 Hz
2.3

@Frequency 60 Hz
ASTM D150
Dielectric Strength 90.0 kV/mm
2290 kV/in
ASTM D149
Dissipation Factor 0.00019

@Frequency 50 Hz
0.00019

@Frequency 50 Hz
ASTM D150