Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.19 - 1.22 g/cc | 0.0430 - 0.0441 lb/in³ | Average value: 1.21 g/cc Grade Count:8 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.09 - 1.22 g/cc | 0.0394 - 0.0441 lb/in³ | Average value: 1.15 g/cc Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.17 - 1.22 g/cc | 0.0424 - 0.0442 lb/in³ | |
Lord Adhesives 202 Semi-Flexible, Fast Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Density | 1.16 - 1.22 g/cc | 0.0419 - 0.0441 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 6221 C GREY The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 54 Flexible PVC, Injection Molding for Footwear Boots - sandshoes |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 61 Flexible PVC, Injection Molding for Footwear Antislip soles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 61/R Flexible PVC, Injection Molding for Footwear Oil resistent bottom boots |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 63 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/F Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/P Flexible PVC, Injection Molding for Footwear Pearl sandals |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/PL Flexible PVC, Injection Molding for Footwear Pearl- perfumed sandals |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 64 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 67 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 69/D Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/AT Flexible PVC, Transparent Extrusion Transparent sheath, UL 94 Class V1 |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/B Flexible PVC, Transparent Extrusion Profiles high transparency |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/K1 Flexible PVC, Transparent Extrusion Transparent embossed profiles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5510 Flexible PVC, Lead Free Gaskets for frames |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 282A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 285A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 382A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 485A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 795A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 482A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 682A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 75/D Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70 Flexible PVC, Transparent Extrusion Transparent profiles and pipes |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 5510 Flexible PVC, Lead Free Profiles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 385A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |