Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.19 - 1.22 g/cc | 0.0430 - 0.0441 lb/in³ | Average value: 1.21 g/cc Grade Count:8 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.09 - 1.22 g/cc | 0.0394 - 0.0441 lb/in³ | Average value: 1.15 g/cc Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.16 - 1.22 g/cc | 0.0419 - 0.0441 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 6221 C GREY The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 54 Flexible PVC, Injection Molding for Footwear Boots - sandshoes |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 61 Flexible PVC, Injection Molding for Footwear Antislip soles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 61/R Flexible PVC, Injection Molding for Footwear Oil resistent bottom boots |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/F Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/P Flexible PVC, Injection Molding for Footwear Pearl sandals |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/PL Flexible PVC, Injection Molding for Footwear Pearl- perfumed sandals |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 64 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 67 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 69/D Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 65/A Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/AT Flexible PVC, Transparent Extrusion Transparent sheath, UL 94 Class V1 |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70/K1 Flexible PVC, Transparent Extrusion Transparent embossed profiles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75/R Flexible PVC, Transparent Extrusion Pipes mixed rubber |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5510 Flexible PVC, Lead Free Gaskets for frames |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 282A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 285A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 382A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 485A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 790A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 795A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 482A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 682A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 75/D Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 70 Flexible PVC, Transparent Extrusion Transparent profiles and pipes |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 5510 Flexible PVC, Lead Free Profiles |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 385A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.18 - 1.22 g/cc | 0.0426 - 0.0441 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |