Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.21 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
PTS Trimid® N6-G13L 13% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Density 1.21 g/cc
0.0437 lb/in³
Polimeri Europa KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber  (discontinued **)
Symbol according to ISO 1043/1/2: PC+ABS (GF) Injection moulding grade, reinforced with 10% glass fibres, high stiffness, very good dimensional stability. Vicat/B50 = 135°C Main application field..
Density 1.21 - 1.43 g/cc
0.0437 - 0.0517 lb/in³
Average value: 1.30 g/cc Grade Count:10
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Density 1.21 - 1.32 g/cc
0.0437 - 0.0477 lb/in³
Average value: 1.27 g/cc Grade Count:8
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
DSM Akulon® K224-HG2U (Dry) 10% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Global GPC-105-S Enhanced Modulus, Structural Grade Polycarbonate
Information provided by Global Polymers Corporation.
Density 1.21 g/cc
0.0437 lb/in³
ISO 2781
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..
Density 1.21 g/cc
0.0437 lb/in³
ISO 2781
Huntsman AVALON® 90 AK Thermoplastic Polyurethane
Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har..
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East)
Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Techmer ES Luriblend® HTN 01420 BK
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppearance: BlackInformation provide..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive.
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP
LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized.
Density 1.21 g/cc
<br>@Temperature 23.0 °C
0.0437 lb/in³
<br>@Temperature 73.4 °F
ASTM D1928
Trelleborg Horda Cable E8406 Easy Strippable Semiconductive Shielding
E8406 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8406 meets the requirements as be..
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183-1
Covestro Makrolon® XT5010 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Easy processing• Low..
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
BASF Elastollan® S80A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Toyobo Pelprene™ S-1001 Polyester TPE
Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block..
Density 1.21 g/cc
0.0437 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Density 1.21 - 1.25 g/cc
0.0437 - 0.0452 lb/in³
ISO R 1183
Fainplast Compounds MGS 75 Medical Flexible PVC, Injection Molding
Connectors and special components
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Albis Plastics Cellulose Acetate Butyrate B9424-3 , 3% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Density 1.21 g/cc
0.0437 lb/in³
3M Novec™ FC-4432 Fluorosurfactant
3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga..
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Owens Corning Glass Fiber Reinforced Polyphenylene Oxide (PPO), 20 wt.% glass
Polyphenylene Oxide provides excellent resistance to aqueous media. It is softened by aromatic hydrocarbons. Data provided by the manufacturer, Owens Corning.
Copyright © lookpolymers.com All Rights Reserved