Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® TPX-PA6-03034 Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name Luriblend®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Techmer ES Luriblend® TPX-PA6-03034 Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 139 MPa
20200 psi
ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149