| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | |
| 1.21 g/cc | 0.0437 lb/in³ | DAM; ISO 1183 | |
| Water Absorption | 6.5 % @Thickness 2.00 mm |
6.5 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Moisture Absorption | 2.20 % @Thickness 2.00 mm |
2.20 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity | 46700 cP @Shear Rate 5000 1/s, Temperature 305 °C |
46700 cP @Shear Rate 5000 1/s, Temperature 581 °F |
ISO 11403-1 -2 |
| 50730 cP @Shear Rate 5000 1/s, Temperature 295 °C |
50730 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 | |
| 55340 cP @Shear Rate 5000 1/s, Temperature 285 °C |
55340 cP @Shear Rate 5000 1/s, Temperature 545 °F |
ISO 11403-1 -2 | |
| 141400 cP @Shear Rate 500 1/s, Temperature 305 °C |
141400 cP @Shear Rate 500 1/s, Temperature 581 °F |
ISO 11403-1 -2 | |
| 157800 cP @Shear Rate 500 1/s, Temperature 295 °C |
157800 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 | |
| 176700 cP @Shear Rate 500 1/s, Temperature 285 °C |
176700 cP @Shear Rate 500 1/s, Temperature 545 °F |
ISO 11403-1 -2 | |
| Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
| Linear Mold Shrinkage, Flow | 0.0050 cm/cm | 0.0050 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 74 | 74 | 50%RH; ISO 2039-2 |
| 90 | 90 | DAM; ISO 2039-2 | |
| Tensile Strength at Break | 67.0 MPa | 9720 psi | 50%RH; ISO 527-1/-2 |
| 118 MPa | 17100 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 4.0 % | 4.0 % | DAM; ISO 527-1/-2 |
| 10 % | 10 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 3.70 GPa | 537 ksi | 50%RH; ISO 527-1/-2 |
| 5.10 GPa | 740 ksi | DAM; ISO 527-1/-2 | |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | DAM; ISO 180/1A |
| 9.00 kJ/m² | 4.28 ft-lb/in² | 50%RH; ISO 180/1A | |
| 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A | |
| 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | 50%RH; ISO 179/1eU |
| 6.70 J/cm² | 31.9 ft-lb/in² | DAM; ISO 179/1eU | |
| 5.40 J/cm² @Temperature -30.0 °C |
25.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| 5.90 J/cm² @Temperature -30.0 °C |
28.1 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | DAM; ISO 179/1eA |
| 1.40 J/cm² | 6.66 ft-lb/in² | 50%RH; ISO 179/1eA | |
| 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
| Tensile Creep Modulus, 1 hour | 4030 MPa @Time 3600 sec |
585000 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
| Tensile Creep Modulus, 1000 hours | 3180 MPa @Time 3.60e+6 sec |
461000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | DAM; ISO 11359-1/-2 |
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 242 °C | 468 °F | DAM; ISO 75-1/-2 |
| Vicat Softening Point | 239 °C | 462 °F | DAM; 50°C/h 50N; ISO 306 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
DAM; IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 250 V | 250 V | DAM; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additives | Lubricants | |
| Delivery Form | Pellets | |
| Odour | class 4 | VDA 270; C3 |
| Processing | Injection Moulding | |
| Regional Availability | Europe | |
| Near East/Africa | ||
| Special Characteristics | Heat stabilised or stable to heat | |
| UL recognition | UL | DAM |