| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible 83700 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
| Volatiles | 1.1 % @Thickness 1.91 mm, Temperature 105 °C |
1.1 % @Thickness 0.0752 in, Temperature 221 °F |
Loss; Method A; ASTM D1203B |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 83 | 83 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 15.2 MPa | 2200 psi | 510 mm/min; ASTM D638 |
| Elongation at Break | 320 % | 320 % | 510 mm/min; ASTM D638 |
| Tear Strength | 57.9 kN/m | 330 pli | Die C, 2 in/min; ASTM D1004 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive Specifications | CHRYSLER MS-DC23 CPN2928 Color: 2850 Black | |
| CHRYSLER MS-DC232 CPN2865 Color: 2850 Black | ||
| FORD ESB-M4D259 Type IV | ||
| FORD ESB-M4D284 Type IV | ||
| FORD ESB-M4D284-C4 Color: Charcoal, Black | ||
| Features | General Purpose | |
| Medium Gloss | ||
| Forms | Pellets | |
| Fungal Resistance | Pass | ASTM G21 |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Low Temperature Flexibility | Pass | -29°C, 508.0 µm; 4 hr, 12 mm |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Automotive Applications | |
| General Purpose | ||
| Outdoor Applications | ||
| Xenon Weatherometer | Pass | SAE J1960; Exterior, 2500 kJ/m², Black, dE*<3.0 |