Polymer Property : Specific Gravity = 1.76 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.76 g/cc
1.76 g/cc
Old Hickory M&M Clays, Inc. Wilco-SLU Kaolin Clay
Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selec..
Specific Gravity 1.76 g/cc
1.76 g/cc
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits..
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
High Melt Viscosity - Polymer for Non-Architectural Dispersion CoatingsInformation provided by Solvay Specialty Polymers.
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
Technetics Group Amicon™ PVDF  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Specific Gravity 1.76 g/cc
1.76 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Specific Gravity 1.76 g/cc
1.76 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF)
LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade
Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s..
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Specific Gravity 1.76 - 1.78 g/cc
1.76 - 1.78 g/cc
ASTM D792
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Gravity 1.76 g/cc
1.76 g/cc
Method A; ASTM D792
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Specific Gravity 1.76 - 1.80 g/cc
1.76 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..