Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine J-2 PVDF Extrusion Grade Description: J-2 PVDF is a kind of granules homopolymer, which has middle melt viscosity, J-2 is more suitable for extrusion process. J-2 PVDF pellets as raw materials, the finished products has exc.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine M-1 PVDF Molding Grade Description: M-1 PVDF is a kind of granules homopolymer, which has high melt viscosity, M-1 is more suitable for compression molding process. M-1 PVDF pellets as raw materials, the finished products.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine T-2 PVDF for Powder Coatings Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine Z-1 PVDF Injection Grade Description: Z-1 PVDF is a kind of granular homopolymer, which has low melt viscosity, Z-1 is more suitable for injection molding. Z-1 PVDF pellets as raw materials, the finished products has excell.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Specific Gravity | 1.76 - 1.79 g/cc | 1.76 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Specific Gravity | 1.73 - 1.79 g/cc | 1.73 - 1.79 g/cc | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, th.. |