Polymer Property : Specific Gravity = 1.77 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
PolyOne Edgetek® SF-35GF-15MC/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled  (discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Specific Gravity 1.77 - 1.78 g/cc
1.77 - 1.78 g/cc
ISO R1183D
Shanghai Ofluorine 9201F PVDF Powder for cables
Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, ..
Specific Gravity 1.77 - 1.78 g/cc
1.77 - 1.78 g/cc
ISO R1183D
Shanghai Ofluorine 9202F PVDF Powder for cables
Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, ..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine M-1 PVDF Molding Grade
Description: M-1 PVDF is a kind of granules homopolymer, which has high melt viscosity, M-1 is more suitable for compression molding process. M-1 PVDF pellets as raw materials, the finished products..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine T-2 PVDF for Powder Coatings
Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Specific Gravity 1.77 g/cc
1.77 g/cc
BYK Cloisite® 20A Nanoclay
Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Gravity 1.77 g/cc
1.77 g/cc
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester
BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 g/cc
1.77 g/cc
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st..
Specific Gravity 1.77 g/cc
1.77 g/cc
ASTM D792
Premix Premi-Glas® 1282-32 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1282-32 VE SMC is an enhanced high strength glass reinforced vinyl ester molding compound formulated for under-the-hood automotive applications. Key features and benefi..
Specific Gravity 1.77 - 1.80 g/cc
1.77 - 1.80 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Specific Gravity 1.77 - 1.78 g/cc
1.77 - 1.78 g/cc
ISO R1183D
Shanghai Ofluorine 9201 PVDF Pellets for cables
Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, ..