| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Valox® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Valox® 780 PBT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.77 g/cc | 1.77 g/cc | ASTM D792 |
| Water Absorption | 0.020 % @Time 86400 sec |
0.020 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm @Thickness 1.50 - 3.20 mm |
0.0030 - 0.0040 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
| 0.0040 - 0.0060 cm/cm @Thickness 3.20 - 4.60 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 - 0.181 in |
SABIC Method | |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Thickness 1.50 - 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.0591 - 0.126 in |
SABIC Method |
| 0.0060 - 0.0080 cm/cm @Thickness 3.20 - 4.60 mm |
0.0060 - 0.0080 in/in @Thickness 0.126 - 0.181 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 116 | 116 | ASTM D785 |
| Tensile Strength at Break | 99.0 MPa | 14400 psi | Type I, 5 mm/min; ASTM D638 |
| Flexural Strength | 165 MPa | 23900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 10.34 GPa | 1500 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D4812 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
14.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 28.8 µm/m-°C @Temperature 60.0 - 138 °C |
16.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 193 °C @Thickness 6.40 mm |
379 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
| Flammability, UL94 | V-0 @Thickness 0.810 mm |
V-0 @Thickness 0.0319 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 3.50e+15 ohm-cm | 3.50e+15 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 3.9 @Frequency 100 Hz |
3.9 @Frequency 100 Hz |
ASTM D150 | |
| Dielectric Strength | 18.1 kV/mm @Thickness 3.20 mm |
460 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
| 25.5 kV/mm @Thickness 1.60 mm |
648 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 | |
| Dissipation Factor | 0.0070 @Frequency 100 Hz |
0.0070 @Frequency 100 Hz |
ASTM D150 |
| 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Specific Volume | 0.56cm^3/g | ASTM D792 |