Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 2.00 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC1000 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade
NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca..
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC1100 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade
NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca..
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC1101 Single-Wall Isolated and Bundled Carbon Nanotubes - Research grade
NANOCYL™ NC1000 series single-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 70% ca..
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC2100 Double-Wall Isolated and Bundled Carbon Nanotubes - Research Grade
NANOCYL™ NC2000 series double-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 90% ca..
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC2101 Double-Wall Isolated and Bundled Carbon Nanotubes - Research Grade
NANOCYL™ NC2000 series double-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 90% ca..
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC3100 Thin Multi-Wall Carbon Nanotubes - Research Grade
NANOCYL™ NC3000 series thin multi-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 95..
Specific Gravity 1.30 - 2.00 g/cc
1.30 - 2.00 g/cc
Nanocyl NANOCYL™ NC3101 Thin Multi-Wall Carbon Nanotubes - Research Grade
NANOCYL™ NC3000 series thin multi-wall carbon nanotubes are produced via the catalytic carbon vapor deposition (CCVD) process. Nanotubes which exit the reactor are then purified to greater than 95..
Specific Gravity 1.60 - 2.00 g/cc
1.60 - 2.00 g/cc
Parker Chomerics CHO-SHIELD® 4076 Conductive Coating
CHO-SHIELD® 4076 nickel-filled polyurethane is recommended for shielding an entire room. This durable coating adheres well to plaster, wood, glass, concrete, drywall and most metals.Information pro..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Parker Chomerics CHO-SHIELD® 4916 Conductive Coating
Conductive CoatingInformation provided by Chomerics
Specific Gravity 1.90 - 2.00 g/cc
1.90 - 2.00 g/cc
ISO 1183
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 6501 DAIP
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 6552 DAIP
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Specific Gravity 1.90 - 2.00 g/cc
1.90 - 2.00 g/cc
ISO 1183
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Specific Gravity 1.90 - 2.00 g/cc
1.90 - 2.00 g/cc
ISO 1183
Raschig Group EPOXIDUR® 3582 EP Epoxy
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi..
Specific Gravity 1.90 - 2.00 g/cc
1.90 - 2.00 g/cc
ASTM D792
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ASTM D792
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Specific Gravity 1.90 - 2.00 g/cc

@Thickness 1.57 mm
1.90 - 2.00 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..
Specific Gravity 1.70 - 2.00 g/cc
1.70 - 2.00 g/cc
IEC 1212-2 8.1
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet
Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe.
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
IEC 1212-2 8.1
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet
Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe.
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound
BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound
BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinfo..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound
BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co..
Specific Gravity 1.90 - 2.00 g/cc
1.90 - 2.00 g/cc
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade
BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Parker Chomerics CHO-BOND 1035 Electrically Conductive Sealant
Electrically conductive, one component RTV silicone which provides both environmental sealing and EMI/RFI shielding. This sealant, filled with silver-plated glass particles, contains no acetic acid,..
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
ISO 1183
Raschig Group 5557 DAP  (discontinued **)
Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h..
Copyright © lookpolymers.com All Rights Reserved