| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA) |
| Manufacturer | Arkema |
| Trade Name | Pebax® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
| Water Absorption | 1.2 % | 1.2 % | 24 hr in water at 20°C; ASTM D570 |
| Water Absorption at Saturation | 0.40 % | 0.40 % | 20°C and 65% RH; ASTM D570 |
| Melt Flow | 9.0 g/10 min | 9.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 42 | 42 | ASTM D2240 |
| Tensile Strength at Break | 36.0 MPa | 5220 psi | ASTM D638 |
| Elongation at Break | 600 % | 600 % | ASTM D638 |
| Flexural Modulus | 0.0780 GPa | 11.3 ksi | ASTM D790 |
| Izod Impact, Notched | NB | NB | ASTM D256-A |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ASTM D256-A | |
| Izod Impact, Unnotched | NB | NB | ASTM D256-A |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ASTM D256-A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 22.0 J/g | 9.46 BTU/lb | ASTM D3417 |
| CTE, linear | 200 µm/m-°C @Temperature -40.0 - 140 °C |
111 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
| Melting Point | 147 °C | 297 °F | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 52.0 °C | 126 °F | ASTM D648 |
| Vicat Softening Point | 114 °C | 237 °F | under 1 daN; ASTM D1525 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 3.00e+12 ohm @Temperature 20.0 °C |
3.00e+12 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |