Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -20.0 °C |
28.6 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 GF 30 PA66 reinforced with glass fiber PA66 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -20.0 °C |
28.6 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S CP400 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
PolyOne Bergamid™ A700 G20 U-SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued ** The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 30 H2.0 EF 901510 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eU |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Barlog Plastics KEBATER BF230 PBT, 30% glass fiber reinforced, food grade PBT-GF30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A RV400 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® B 3235 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, improved flowability |