| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
1.50
-
8.00
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
0.714
-
3.81
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 2.58 kJ/m² Grade Count:6 |
|
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| Izod Impact, Notched (ISO) |
1.50
-
8.00
kJ/m² <br>@Thickness 4.00 - 4.00 mm
|
0.714
-
3.81
ft-lb/in² <br>@Thickness 0.157 - 0.157 in
|
Average value: 2.58 kJ/m² Grade Count:6 |
|
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| Izod Impact, Notched (ISO) | 1.50 - 10.0 kJ/m² | 0.714 - 4.76 ft-lb/in² | Average value: 6.68 kJ/m² Grade Count:11 |
|
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
|
|||
| Izod Impact, Notched (ISO) | 1.50 - 8.00 kJ/m² | 0.714 - 3.81 ft-lb/in² | Average value: 4.30 kJ/m² Grade Count:30 |
|
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Izod Impact, Notched (ISO) | 1.50 kJ/m² | 0.714 ft-lb/in² | ISO 180-93 |
|
Wellman Wellamid® GS1684-WBK1 25% Glass Sphere Filled Nylon 66
Description: Glass Sphere Filled Nylon 66Information provided by Wellman.
|
|||
| Izod Impact, Notched (ISO) | 1.50 kJ/m² | 0.714 ft-lb/in² | ASTM D256 |
|
Total PSC 1441 Easy Flow, High Heat Resistance Polystyrene
Total Petrochemicals Polystyrene 1441 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle time..
|
|||
| Izod Impact, Notched (ISO) | 1.50 kJ/m² | 0.714 ft-lb/in² | ISO 180/A |
|
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
|
|||
| Izod Impact, Notched (ISO) | 1.50 kJ/m² | 0.714 ft-lb/in² | ISO 180/A |
|
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN
Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Izod Impact, Notched (ISO) | 1.50 kJ/m² | 0.714 ft-lb/in² | ISO 180/A |
|
Styrolution Luran® 348 Q Transparent SAN
Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Izod Impact, Notched (ISO) | 1.50 kJ/m² - NB | 0.714 ft-lb/in² - NB | Average value: 27.7 kJ/m² Grade Count:10 |
|
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
|
|||