| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 2.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.50 kJ/m² Grade Count:4 |
| Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
| Izod Impact, Notched (ISO) | 4.00 - 10.0 kJ/m² | 1.90 - 4.76 ft-lb/in² | Average value: 8.01 kJ/m² Grade Count:11 |
| Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
| Izod Impact, Notched (ISO) | 5.00 - 10.0 kJ/m² @Temperature -40.0 - 30.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 6.99 kJ/m² Grade Count:21 |
| Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
| Izod Impact, Notched (ISO) | 9.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
4.28 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.67 kJ/m² Grade Count:3 |
| Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
| Izod Impact, Notched (ISO) | 6.00 - 10.0 kJ/m² | 2.86 - 4.76 ft-lb/in² | Average value: 7.91 kJ/m² Grade Count:11 |
| Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
| Izod Impact, Notched (ISO) | 1.70 - 10.0 kJ/m² | 0.809 - 4.76 ft-lb/in² | Average value: 3.22 kJ/m² Grade Count:13 |
| Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
| Izod Impact, Notched (ISO) | 1.50 - 10.0 kJ/m² | 0.714 - 4.76 ft-lb/in² | Average value: 6.68 kJ/m² Grade Count:11 |
| Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
| Izod Impact, Notched (ISO) | 3.00 - 10.0 kJ/m² | 1.43 - 4.76 ft-lb/in² | Average value: 6.86 kJ/m² Grade Count:14 |
| Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
| Izod Impact, Notched (ISO) | 4.00 - 10.0 kJ/m² | 1.90 - 4.76 ft-lb/in² | Average value: 6.84 kJ/m² Grade Count:36 |
| Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
| Izod Impact, Notched (ISO) | 4.00 - 10.0 kJ/m² @Temperature -30.0 - 0.000 °C |
1.90 - 4.76 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 6.80 kJ/m² Grade Count:9 |
| Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
| Izod Impact, Notched (ISO) | 3.00 - 10.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 6.70 kJ/m² Grade Count:14 |
| Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
| Izod Impact, Notched (ISO) | 3.90 - 10.0 kJ/m² | 1.86 - 4.76 ft-lb/in² | Average value: 7.17 kJ/m² Grade Count:8 |
| Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
| Izod Impact, Notched (ISO) | 4.00 - 10.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.90 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 7.31 kJ/m² Grade Count:4 |
| Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
| Izod Impact, Notched (ISO) | 3.00 - 10.0 kJ/m² @Temperature -40.0 - -30.0 °C |
1.43 - 4.76 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 5.65 kJ/m² Grade Count:15 |
| Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
| Izod Impact, Notched (ISO) | 6.50 - 10.0 kJ/m² | 3.09 - 4.76 ft-lb/in² | Average value: 8.09 kJ/m² Grade Count:4 |
| Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
| Izod Impact, Notched (ISO) | 3.00 - 10.0 kJ/m² | 1.43 - 4.76 ft-lb/in² | Average value: 5.65 kJ/m² Grade Count:21 |
| Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
| Izod Impact, Notched (ISO) | 3.00 - 10.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 5.09 kJ/m² Grade Count:9 |
| Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
| Izod Impact, Notched (ISO) | 2.00 - 10.0 kJ/m² @Temperature -30.0 - -20.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.11 kJ/m² Grade Count:9 |
| Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
| Izod Impact, Notched (ISO) | 5.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.50 kJ/m² Grade Count:2 |
| Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
| Izod Impact, Notched (ISO) | 4.00 - 10.0 kJ/m² @Temperature -40.0 - 0.000 °C |
1.90 - 4.76 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 7.70 kJ/m² Grade Count:29 |
| Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
| Izod Impact, Notched (ISO) | 7.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.07 kJ/m² Grade Count:7 |
| Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
| Izod Impact, Notched (ISO) | 7.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.33 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 8.00 kJ/m² Grade Count:3 |
| Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
| Izod Impact, Notched (ISO) | 8.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
3.81 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.33 kJ/m² Grade Count:2 |
| Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
| Izod Impact, Notched (ISO) | 10.0 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
4.76 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 10.0 kJ/m² Grade Count:1 |
| Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||
| Izod Impact, Notched (ISO) | 2.00 - 10.0 kJ/m² @Temperature -30.0 - -20.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 7.11 kJ/m² Grade Count:9 |
| Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
| Izod Impact, Notched (ISO) | 2.00 - 10.0 kJ/m² | 0.952 - 4.76 ft-lb/in² | Average value: 4.33 kJ/m² Grade Count:9 |
| Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
| Izod Impact, Notched (ISO) | 3.00 - 10.0 kJ/m² @Temperature -30.0 - -30.0 °C |
1.43 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 kJ/m² Grade Count:4 |
| Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||