Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a .. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 2mm/min; ISO 178 |
Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco 5482 Phenolic, Granular, Injection Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
Plenco 7591 Phenolic, Briquette, Injection Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
Eurostar Staramide RF006S-GY9A121 PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006S-GY9A121 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0069 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding Resin (also known as Starflam PA6 30E6 Z88)Information provided by Eurostar. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D 790 |
Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Conditioned) Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 114 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | dry; ISO 178 |
DSM Stanyl® TQ261F5 PA46-GF25 25% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East) LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GFL36 PSU (Europe-Africa-Middle East) LNP* Lubricomp* GFL36 is a compound based on Polysulfone resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |