| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | BASF |
| Trade Name | Ultramid® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
| Water Absorption | 5.9 - 6.5 % | 5.9 - 6.5 % | ISO 62 |
| Moisture Absorption at Equilibrium | 1.8 - 2.2 % | 1.8 - 2.2 % | 23°C/50% R.H.; ISO 62 |
| Viscosity Measurement | 160 | 160 | Viscosity Number; ISO 307 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | |
| Melt Flow | 33.25 g/10 min @Load 5.00 kg, Temperature 275 °C |
33.25 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 150 MPa | 21800 psi | 50mm/min; ISO 527 |
| Elongation at Yield | 3.6 % | 3.6 % | 50mm/min; ISO 527 |
| Modulus of Elasticity | 9.00 GPa | 1310 ksi | ISO 527 |
| Flexural Strength | 220 MPa | 31900 psi | ISO 178 |
| Flexural Modulus | 7.40 GPa | 1070 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/A |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A | |
| Charpy Impact Unnotched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 178 |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eU |
| 9.50 J/cm² | 45.2 ft-lb/in² | ISO 179/1eA | |
| 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 - 25.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
11.1 - 13.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 60.0 - 70.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 38.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
| Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 220 °C | 428 °F | DIN 53765 |
| Maximum Service Temperature, Air | 180 °C | 356 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ISO 75 |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dissipation Factor | 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 550 V | 550 V | Test Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 270 - 290 °C | 518 - 554 °F | Injection-molding/Extrusion |
| Mold Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection-molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | BK30564 | |
| Commercial Status | North America and Europe | |
| Impact Modified | Yes | |
| Primary Processing Technique | Injection Molding |