Polymer Property : Glass Transition Temp, Tg = -38.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Glass Transition Temp, Tg -40.0 - -38.0 °C

@Frequency 1.00 Hz
-40.0 - -36.4 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..