| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
|
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | TMA |
|
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant
LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC, 50°F/min; DIN 51.007 |
|
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer
PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
|
Seals Eastern 7065 Neoprene / Chloroprene
General purpose neopreneInformation provided by Seals Eastern, Inc.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
|
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF)
Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
|
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF)
Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
|
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Ultra High ViscosityUses: Batteries; BinderAdditio..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
|
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
|
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM ..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D3418 |
|
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
|
Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
|
Wanhua Chemical Wanthane® WHT-A890 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
|
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
|
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
|
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
|
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer
3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400Z are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are des..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
|
3M Dyneon™ LTFE 6400ZC Low Temperature Fluoroelastomer
3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400ZC are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are de..
|
|||
| Glass Transition Temp, Tg |
-40.0
-
-38.0
°C <br>@Frequency 1.00 Hz
|
-40.0
-
-36.4
°F <br>@Frequency 1.00 Hz
|
DMA |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Glass Transition Temp, Tg |
-40.0
-
-38.0
°C <br>@Frequency 1.00 Hz
|
-40.0
-
-36.4
°F <br>@Frequency 1.00 Hz
|
DMA |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Glass Transition Temp, Tg |
-40.0
-
-38.0
°C <br>@Frequency 1.00 Hz
|
-40.0
-
-36.4
°F <br>@Frequency 1.00 Hz
|
DMA |
|
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
|
|||
| Glass Transition Temp, Tg |
-40.0
-
-38.0
°C <br>@Frequency 1.00 Hz
|
-40.0
-
-36.4
°F <br>@Frequency 1.00 Hz
|
DMA |
|
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Glass Transition Temp, Tg |
-40.0
-
-38.0
°C <br>@Frequency 1.00 Hz
|
-40.0
-
-36.4
°F <br>@Frequency 1.00 Hz
|
DMA |
|
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
|
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
|
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
|
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | Pellet sample |
|
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
|
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
|
Sorbothane Polyurethane Damping Material, 70 Durometer
Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat..
|
|||
| Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | 10°C/min |
|
Arkema Group Kynar® 4000 HD PVDF
(discontinued **)
Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b..
|
|||