Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 438E0V16304 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 4%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 8%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 375E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 15.0 - 17.0 µm/m-°C @Temperature 1000 °C |
8.33 - 9.44 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-309NM,Insert Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate Plasticizer 8%. Weight loss on heating = 0.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Acetate 109E3V36324 Clear, Trsp Cellulose Acetate
(discontinued **) Plasticizer 24%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate
(discontinued **) Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 15.0 - 17.0 µm/m-°C | 8.33 - 9.44 µin/in-°F | IPC TM-650 2.4.41 |
Arlon 47N Quick Cure Epoxy Low-Flow Prepreg 47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate