Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 428 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Processing Temperature <= 220 °C
<= 428 °F
Premix Thermoplastics PRE-ELEC® ESD 6020 Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 6020 is a dissipative masterbatch developed for coextruded HIPS-sheets. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent static dissipative pro..
Processing Temperature 220 - 250 °C
428 - 482 °F
Recommended injection moulding temperature
Reliance Industries Relene M60075 Polyethylene
Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade..
Processing Temperature <= 220 °C
<= 428 °F
PolyChem Alloy PolySept 2007A
PolySept products typically contain 5 – 20% of an antimicrobial agent that is compounded into a plastic resin. The result is an antimicrobial polymer concentrate in a uniform pelletized form. PolyS..
Processing Temperature 220 °C
428 °F
Post cure, 2 hours
Mitsui MILEXâ„¢ XL-225MB Phenol Aralkyl Resin, Standard Grade
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Processing Temperature 220 °C
428 °F
Post cure, 2 hours
Mitsui MILEXâ„¢ XL-325M Phenol Aralkyl Resin, High Molecular Weight
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Processing Temperature 220 °C
428 °F
Shinil Chemical SHINSTRA PP (SM400) Structural Polymer Household
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EE168AI Polypropylene TPO Compound
Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EE260AI Polypropylene TPO Compound
Daplen™ EE260AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EH104AE Polypropylene TPO Compound
Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis PS65C40 Polypropylene Compound, Mineral Filled
PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and..
Processing Temperature 220 - 250 °C
428 - 482 °F
Zhejiang Juner PA-A6 GF20%
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Processing Temperature 220 - 250 °C
428 - 482 °F
Zhejiang Juner PA-A6-4 Non-Reinforced
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Processing Temperature 220 °C
428 °F
C3
UBE 7024B Five Layer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EE188AI Polypropylene TPO Compound
Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF261AI Polypropylene TPO Compound
Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF267AI Polypropylene TPO Compound
Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Processing Temperature 220 - 240 °C
428 - 464 °F
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 220 - 250 °C
428 - 482 °F
Extrusion Range
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Processing Temperature 220 - 230 °C
428 - 446 °F
Injection
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 220 - 230 °C
428 - 446 °F
Injection
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 220 - 270 °C
428 - 518 °F
Resin Temperature
Asahi Kasei Xyron® 240W Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Processing Temperature 220 - 270 °C
428 - 518 °F
Resin Temperature
Asahi Kasei Xyron® 340W Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Processing Temperature 220 - 250 °C
428 - 482 °F
Extrusion Range
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Processing Temperature 220 - 270 °C
428 - 518 °F
Resin Temperature
Asahi Kasei Xyron® 300V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF103AE Polypropylene TPO Compound
Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an..
Processing Temperature 220 °C
428 °F
Typical extrusion metering zone. Do not exceed 238°C (460°F).
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin
Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc..
Copyright © lookpolymers.com All Rights Reserved