Processing Properties Metric English Comments
Processing Temperature 220 - 235 °C
428 - 455 °F
Barrel Temperature
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde..
Processing Temperature <= 220 °C
<= 428 °F
Premix Thermoplastics PRE-ELEC® ESD 4000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive
PRE-ELEC® ESD 4000 is a polyolefin compatible dissipative masterbatch developed for PELD and PE-HD film, sheet, blow and injection moulded products. The active substance is an IDP (inherently dissi..
Processing Temperature <= 220 °C
<= 428 °F
PolyChem Alloy PolySept 2007A
PolySept products typically contain 5 – 20% of an antimicrobial agent that is compounded into a plastic resin. The result is an antimicrobial polymer concentrate in a uniform pelletized form. PolyS..
Processing Temperature 220 - 260 °C
428 - 500 °F
Average value: 240 °C Grade Count:20
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Processing Temperature 220 - 270 °C
428 - 518 °F
IRPC Polimaxx Porene KU200 Acrylonitrile Butadiene Styrene
Applications:extrusion applicationautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances
Processing Temperature 220 °C
428 °F
Post cure, 2 hours
Mitsui MILEXâ„¢ XL-225MB Phenol Aralkyl Resin, Standard Grade
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Processing Temperature 220 - 230 °C
428 - 446 °F
C2
UBE 5034FDX33 Air Blown Nylon 6/66 Film
Specialties: High transparencyLow neck-inNucleated typeApplications: Suitable for T-die,Water and Air blown process Processing: Shrink bags (Water) Pouch ( Air blown) Information provided by UBE.
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EE108U Polypropylene TPO Compound
Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF005AE Polypropylene TPO Compound
Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF210AE Polypropylene TPO Compound
Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Processing Temperature 220 - 240 °C
428 - 464 °F
Total HDPE SB 1461 High Density Polyethylene - Injection Stretch Blow Molding
HDPE SB 1461 is a high density polyethylene with very high stiffness. It has been specifically designed for the manufacture of thin walled containers for foodstuffs (dairy applications particularly..
Processing Temperature 220 - 250 °C
428 - 482 °F
Zhejiang Juner PA-A6-4 Non-Reinforced
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Processing Temperature 220 °C
428 °F
C2
UBE 7024B Five Layer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF261AI Polypropylene TPO Compound
Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
Processing Temperature 220 - 240 °C
428 - 464 °F
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Processing Temperature 220 - 290 °C
428 - 554 °F
E-Polymers Tekaloy® G70A3 , Heat Resistance, Easy Molding PC/ABS Alloy
Heat Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd.
Processing Temperature 220 °C
428 °F
Recommended Extrusion Temperature
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Processing Temperature 220 °C
428 °F
Recommended Extrusion Temperature
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Processing Temperature 220 - 250 °C
428 - 482 °F
Extrusion Range
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Processing Temperature 220 °C
428 °F
Recommended Extrusion Temperature
Arkema Group Pebax® MX 1205 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MX 1205 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to mee..
Processing Temperature 220 °C
428 °F
Recommended Extrusion Temperature
Arkema Group Pebax® Rnew 40R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 40R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Processing Temperature 220 - 270 °C
428 - 518 °F
Resin Temperature
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Processing Temperature 220 - 270 °C
428 - 518 °F
Resin Temperature
Asahi Kasei Xyron® 340W Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Processing Temperature 220 - 250 °C
428 - 482 °F
Resin Temperature
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
Processing Temperature <= 220 °C
<= 428 °F
Addcomp ADD-VANCE® SA 420 Slip/anti-block additive
Fields of application: Improves slip and anti-block properties of thermoplastics. It can also be used as a release agent for injection molded products.Examples: (L)LDPE, HDPE, PP, PS, HIPS, TPO, ABS..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis Daplen™ EF103AE Polypropylene TPO Compound
Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an..
Processing Temperature 220 - 260 °C
428 - 500 °F
mass temperature
Borealis MD231U Polypropylene Compound, Mineral Filled
MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc..
Processing Temperature 220 - 290 °C
428 - 554 °F
E-Polymers Tekaloy® G70A2 Impact Resistance, Easy Molding PC/ABS Alloy
Impact Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd.