| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Die Temperature | 220 °C | 428 °F | Zone 3 |
|
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
|
|||
| Die Temperature | 220 °C | 428 °F | Zone 3 |
|
Premix Thermoplastics PRE-ELEC® PE 1291
PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
|
|||
| Die Temperature | 220 °C | 428 °F | Zone 3 |
|
Premix Thermoplastics PRE-ELEC® PP 1386
PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
|
|||
| Die Temperature | 220 °C | 428 °F | Zone 3 |
|
Premix Thermoplastics PRE-ELEC® PS 1324
PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
|
|||
| Die Temperature | 220 °C | 428 °F | Zone 3 |
|
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
|
|||
| Die Temperature | 220 °C | 428 °F | Zone 3 |
|
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
|
|||
| Die Temperature | 220 - 250 °C | 428 - 482 °F | Average value: 238 °C Grade Count:6 |
|
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
|
|||
| Die Temperature | 220 °C | 428 °F | Blow Molding |
|
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
|
|||
| Die Temperature | 220 °C | 428 °F | |
|
LG Chemical BM662B ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica..
|
|||
| Die Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Die Temperature | 220 - 255 °C | 428 - 491 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT HB9255D Ester Type TPE
Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
|
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
|
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
|
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Die Temperature | 220 - 230 °C | 428 - 446 °F | 6 |
|
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
|
|||
| Die Temperature | 220 - 230 °C | 428 - 446 °F | TIP, 7 |
|
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
|
|||
| Die Temperature | 220 °C | 428 °F | |
|
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
|
|||
| Die Temperature | 220 °C | 428 °F | Blow Film |
|
DuPont Appeel® LSR11D542 Lidding Sealant Resin
Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten..
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene
OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between..
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene
OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe ..
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene
OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC..
|
|||
| Die Temperature | 220 - 240 °C | 428 - 464 °F | |
|
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene
OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA..
|
|||
| Die Temperature | 220 - 250 °C | 428 - 482 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..
|
|||