Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 428 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 220 °C
428 °F
Zone 3
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
Die Temperature 220 °C
428 °F
Zone 3
Premix Thermoplastics PRE-ELEC® PE 1294
PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Die Temperature 220 °C
428 °F
Zone 3
Premix Thermoplastics PRE-ELEC® PS 1324
PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Die Temperature 220 °C
428 °F
Zone 3
Premix Thermoplastics PRE-ELEC® CP 1318  (discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
Die Temperature 220 - 250 °C
428 - 482 °F
Average value: 238 °C Grade Count:6
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Die Temperature 220 °C
428 °F
Blow Molding
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Die Temperature 220 - 250 °C
428 - 482 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1068D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 260 °C
428 - 500 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 260 °C
428 - 500 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 260 °C
428 - 500 °F
Extrusion Molding
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 255 °C
428 - 491 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Die Temperature 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Die Temperature 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Die Temperature 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Die Temperature 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Die Temperature 220 - 240 °C
428 - 464 °F
Extrusion
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Die Temperature 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Die Temperature 220 °C
428 °F
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Die Temperature 220 - 230 °C
428 - 446 °F
Solvay TECHNYL® C 442 Black V PA6, DRY
Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha..
Die Temperature 220 °C
428 °F
Borealis Borcell™ HE4873 High Density Polyethylene
Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foa..
Die Temperature 220 °C
428 °F
Blow Film
DuPont Appeel® LSR11D542 Lidding Sealant Resin
Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten..
Die Temperature 220 - 240 °C
428 - 464 °F
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene
OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between..
Die Temperature 220 °C
428 °F
Extrusion
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer
Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Die Temperature 220 - 240 °C
428 - 464 °F
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene
OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC..
Die Temperature 220 - 240 °C
428 - 464 °F
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene
OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA..
Die Temperature 220 - 240 °C
428 - 464 °F
Average value: 230 °C Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Die Temperature 220 - 250 °C
428 - 482 °F
Extrusion Molding
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..
Copyright © lookpolymers.com All Rights Reserved