| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Die Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
| LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
| Die Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Die Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Die Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
| LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
| LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Die Temperature | 220 - 230 °C | 428 - 446 °F | 6 |
| Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
| Die Temperature | 220 - 230 °C | 428 - 446 °F | TIP, 7 |
| Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
| Die Temperature | 220 - 230 °C | 428 - 446 °F | |
| Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
| Die Temperature | 210 - 230 °C | 410 - 446 °F | |
| Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
| Die Temperature | 215 - 230 °C | 419 - 446 °F | |
| Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | |
| Borealis BB412E Polypropylene Block Copolymer for extrusion and injection BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren.. |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | |
| Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging.
The materia.. |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | |
| Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured.. |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | |
| Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | |
| Borealis HA104E Polypropylene Homopolymer HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica.. |
|||
| Die Temperature | 190 - 230 °C | 374 - 446 °F | Hotmelt Coating Slot Die |
| EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
| Die Temperature | 190 - 230 °C | 374 - 446 °F | Hotmelt Coating Slot Die |
| EMS-Griltech Griltex® D 1377E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
| Die Temperature | 190 - 230 °C | 374 - 446 °F | Hotmelt Coating Slot Die |
| EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
| Die Temperature | 180 - 230 °C | 356 - 446 °F | |
| Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline .. |
|||
| Die Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
| LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||