| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black
Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black
Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black
Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural
Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade
Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural
Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
|
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
|
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom..
|
|||
| Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
|
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products HP532-00 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Natural
Applications: Interior trimCenter tail light bezelPackage trayInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1047D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
|
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
|
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
|
LTL Color Compounds ColorFast® FRA203 ABS
Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
|
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled
For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc.
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Pipe Extrusion |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black
Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
|
RheTech Products M20P101-01 20% Mica Reinforced Polypropylene, Black
Applications: Radiator air bafflesHVAC ductworkClose-out and filler panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||