Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
Polymer Resources ABS-FR1 ABS, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 182 - 221 °C | 360 - 430 °F | |
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High.. |
|||
Front Barrel Temperature | 182 - 221 °C | 360 - 430 °F | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Front Barrel Temperature | 182 - 221 °C | 360 - 430 °F | |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Front Barrel Temperature | 188 - 221 °C | 370 - 430 °F | |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Front Barrel Temperature | 188 - 221 °C | 370 - 430 °F | |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Front Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Front Barrel Temperature | 188 - 221 °C | 370 - 430 °F | |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Front Barrel Temperature | 188 - 221 °C | 370 - 430 °F | |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Front Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |
|||
Front Barrel Temperature | 188 - 221 °C | 370 - 430 °F | |
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
LTL Color Compounds ColorFast® FRA202 General Purpose ABS General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
LTL Color Compounds ColorFast® FRA204 ABS High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
LTL Color Compounds ColorFast® FRA205 ABS Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 204 - 221 °C | 399 - 430 °F | |
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Front Barrel Temperature | 204 - 221 °C | 399 - 430 °F | |
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Front Barrel Temperature | 204 - 221 °C | 399 - 430 °F | |
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Front Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Front Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |