Polymer Property : Front Barrel Temperature = 221 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-FR1 ABS, Flame Retardant
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 182 - 221 °C
360 - 430 °F
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High..
Front Barrel Temperature 182 - 221 °C
360 - 430 °F
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - ..
Front Barrel Temperature 182 - 221 °C
360 - 430 °F
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - ..
Front Barrel Temperature 188 - 221 °C
370 - 430 °F
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Front Barrel Temperature 188 - 221 °C
370 - 430 °F
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Front Barrel Temperature 199 - 221 °C
390 - 430 °F
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl..
Front Barrel Temperature 188 - 221 °C
370 - 430 °F
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Front Barrel Temperature 188 - 221 °C
370 - 430 °F
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Front Barrel Temperature 199 - 221 °C
390 - 430 °F
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl..
Front Barrel Temperature 188 - 221 °C
370 - 430 °F
Fiberfil® PP-60/FR Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
LTL Color Compounds ColorFast® FRA202 General Purpose ABS
General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
LTL Color Compounds ColorFast® FRA203 ABS
Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
LTL Color Compounds ColorFast® FRA204 ABS
High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 210 - 221 °C
410 - 430 °F
LTL Color Compounds ColorFast® FRA205 ABS
Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 204 - 221 °C
399 - 430 °F
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Front Barrel Temperature 204 - 221 °C
399 - 430 °F
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Front Barrel Temperature 204 - 221 °C
399 - 430 °F
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Front Barrel Temperature 199 - 221 °C
390 - 430 °F
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties..
Front Barrel Temperature 199 - 221 °C
390 - 430 °F
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen..